Your finger get tired :BigGrin: It's looking better!
What is “filler primer”? Is that like special thick primer of some kind?[url=https://classicgoldwings.com/forum/viewtopic.php?p=215980#p215980:1ti7giy4 said:mcgovern61 » Today, 7:48 am[/url]":1ti7giy4]
Wet sanding with 400 really smooths everything out. Fixed the Bondo areas, self etching primer again on the small exposed metal post sanding and 2 more coats of filler primer. Wet Sanding later today with 600 grit.
:good:[url=https://classicgoldwings.com/forum/viewtopic.php?p=215998#p215998:3rmp0tc8 said:mcgovern61 » Wed Mar 04, 2020 12:56 am[/url]":3rmp0tc8]
Once these parts are sealed I will start working on the shelter. I spent all of this time on the other parts mostly as a test bed to see what needed to be done to achieve the desired results. The shelter is the most readily viewed painted part on the bike and I wanted to be sure it would be perfect. I certainly did not want to practice these processes on the largest part! :hihihi: